Recommended Cutting Data
Turning – Carbide
coated
ISO Material
Cutting speed Vc [m/min]
ca. 0,15% C
350 - 220 - 380 220 - 380 200 - 340 170 - 220 180 - 230 - - 220 - 320 180 - 230 180 - 230
Unalloyed steel and cast steel
ca. 0,45% C
650 - 190 - 330 190 - 330 180 - 290 160 - 180 170 - 190 - - 180 - 290 170 - 190 170 - 190
ca. 0,75% C
1000 - 160 - 280 160 - 280 150 - 240 120 - 140 130 - 150 - - 150 - 250 130 - 150 130 - 150
600 - 180 - 300 180 - 300 170 - 260 160 - 180 170 - 190 - - 180 - 280 170 - 190 170 - 190
P Low alloyed steel and cast steel
900 - 160 - 260 160 - 260 150 - 240 80 - 140 90 - 150 - - 170 - 250 90 - 150 90 - 150
1200 - 120 - 220 120 - 220 120 - 220 60 - 120 70 - 130 - - 150 - 220 70 - 130 70 - 130
High alloyed steel, high alloyed
tool steel and cast steel
annealed
hardened and tempered
700 - 140 - 220 140 - 220 140 - 200 110 - 190 120 - 200 - - 80 - 160 120 - 200 120 - 200
1100 - 70 - 130 70 - 130 70 - 120 40 - 90 50 - 100 - - 40 - 130 50 - 100 50 - 100
Stainless steel and cast steel
ferritic / martensitic, annealed
martensitic, hardened and tempered
700
1000
- 140 - 220 140 - 220 140 - 220 130 - 170 140 - 180 -
- 70 - 130 70 - 130 70 - 110 100 - 150 110 - 140 -
- 60 - 180 140 - 180 140 - 180
- 40 - 140 110 - 140 110 - 140
M Stainless steel and cast steel
austenitic and austenitic/ferritic
chilled
450 - 600
-
-
-
- 100 - 180 100 - 180 120 - 200 100 - 140 80 - 160 120 - 200 120 - 200
600 - 900
-
-
-
- 70 - 140 70 - 140 70 - 180 70 - 140 40 - 130 90 - 160 90 - 160
pearlitic, ferritic
500 - 700 150 - 210 250 - 380 250 - 380 250 - 340 - - - - 180 - 300 - 120 - 160
Cast iron
pearlitic, martensitic
700 - 850 220 - 350 190 - 300 190 - 300 190 - 250 - - - - 160 - 280 - 90 - 130
K Cast iron with nodular graphite
ferritic
pearlitic
800 - 1100 - - - - - -
120 - 240 -
-
550 220 - 380 220 - 300 220 - 300 200 - 260 - - - - 140 - 230 - 120 - 160
800 200 - 350 150 - 230 150 - 230 150 - 200 - - - - 120 - 170 - 120 - 180
Malleable cast iron
ferritic
pearlitic
450 200 - 400 200 - 300 200 - 300 200 - 260 - - - - 150 - 210 - 140 - 220
750 180 - 320 170 - 230 170 - 230 170 - 200 - - - - 150 - 210 - 110 - 160
Aluminum alloys, long chipping
not heat treatable
heat treatable, heat treated
200 - - - - - - - - - - -
350 - - - - - - - - - - -
12% Si, hardened
250 - - - - - - - - - - -
Casted aluminum alloys
12% Si, heat treatable, hardened 300 - - - - - - - - - - -
12% Si, not heat treatable
450 - - - - - - - - - - -
N
Copper and copper alloys
(brass / bronze)
Lead alloys, Pb > 1%
Brass, bronze
Aluminum bronze
400 - - - - - - - - 200 - 500 - -
300 - - - - - - - - 200 - 500 - -
500 - - - - - - - - 160 - 450 - -
Copper and electrolyte copper
200 - - - - - - - - 100 - 320 - -
Duroplastics
- - - - - - - - 160 - 600 - -
Non-ferrous materials
Reinforced plastics
- - - - - - - - 100 - 300 - -
Hard rubber
-----------
Fe-alloyed annealed
700 - - - - 20 - 40 20 - 40 - - 20 - 60 - 20 - 50
Fe-alloyed hardened
950 - - - - 15 - 35 15 - 35 - - 20 - 60 - 20 - 50
High temperature resistant alloys Ni- oder Co- based annealed
800 - - - - 8 - 25 8 - 25 - - 15 - 50 - 15 - 40
S Ni- oder Co- based casting
1100 - - - - 4 - 15 4 - 15 - - 15 - 40 - 10 - 25
i Titanium alloys, high strength
Ni- oder Co- based hardened
Pure titanium
1200 - - - - 4 - 15 4 - 15 - - 15 - 40 - 20 - 35
500 - 700
-
-
-
- 80 - 130 80 - 130 -
- 90 - 180 - 80 - 140
Alpha- and beta-alloys, hardened
700 - 1000 - - - - 15 - 35 15 - 35 - - 40 - 80 - 25 - 45
Hardened steel
H Hard cast iron
hardened and tempered
hardened and tempered
casting
1000 - 1350 - - - - - - - - 30 - 50 - -
1350 - 1700 - - - - - - - - 10 - 25 - -
1350 - - - - - - - - - 40 - 70 - -
Hardened cast iron
hardened and tempered
1900 - - - - - - - - 10 - 25 - -
The datas cutting speeds given are approximate values.
It is necessary to adjust them to the individual machining operation.
More grades on the
following pages.
450 ARNO®-Werkzeuge | Drehen | Turning | Точение